SAE AMS5707P PDF

$39.00

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 57Ni – 19.5Cr – 13.5Co – 4.3Mo – 3.0Ti – 1.4Al – 0.05Zr – 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated

SAE International , 03/23/2023

File Format: PDF